Performance and wear analysis in machining of Co-based Haynes 25/L605 superalloy using sustainable cooling/lubrication agencies
Yazarlar (8)
Prof. Dr. Murat SARIKAYA Sinop Üniversitesi, Türkiye
Prof. Dr. Çağrı Vakkas Yıldırım Erciyes Üniversitesi, Türkiye
Doç. Dr. Şenol Şirin Düzce Üniversitesi, Türkiye
Arş. Gör. Muhammed Ikbal Kara Erciyes Üniversitesi, Türkiye
Doç. Dr. Emine Şirin Düzce Üniversitesi, Türkiye
Turgay Kıvak Düzce Üniversitesi, Türkiye
Grzegorz M. Królczyk Opole University Of Technology, Polonya
Akın Ataş
The University Of Manchester, İngiltere
Makale Türü Açık Erişim Özgün Makale (SSCI, AHCI, SCI, SCI-Exp dergilerinde yayınlanan tam makale)
Dergi Adı Sustainable Materials and Technologies (Q1)
Dergi ISSN 2214-9929
Dergi Tarandığı Indeksler SCI-Expanded
Makale Dili Türkçe Basım Tarihi 04-2025
Cilt / Sayı / Sayfa 43 / 1 / – DOI 10.1016/j.susmat.2025.e01268
Makale Linki https://doi.org/10.1016/j.susmat.2025.e01268
UAK Araştırma Alanları
Üretim Teknolojileri Triboloji Eklemeli İmalat
Özet
The cobalt-based Haynes 25 superalloy is a key material in sectors such as aerospace, medical, and energy, known for its outstanding high-temperature strength, wear and corrosion resistance. However, its low thermal conductivity and rapid work hardening rate make it inherently difficult to machine, highlighting the need for new cooling and lubrication methods. This work investigates the machinability of Haynes 25 under various sustainable cooling and lubrication techniques, including dry conditions, minimum quantity lubrication (MQL), nanofluids, and cryogenic CO₂. Additionally, hybrid systems combining cryogenic CO₂ with nanofluids are also being investigated. The effectiveness of these approaches was ascertained by thorough investigations of surface roughness, cutting temperature, tool wear, and its mechanisms, and power consumption.Experimental results show that hybrid cooling systems especially …
Anahtar Kelimeler
Co-based Haynes 25 | Hybrid cooling/lubrication systems | Power consumption | Surface roughness | Tool wear | Wear mechanisms