Parametric optimization and process capability analysis for machining of nickel-based superalloy
Yazarlar (10)
Munish Kumar Gupta
Chandigarh University, Hindistan
Mozammel Mia
Ahsanullah University Of Science And Technology, Bangladeş
Catalin I. Pruncu
Imperial College London, İngiltere
Wojciech Kapłonek
Politechnika Koszalinska, Polonya
Krzysztof Nadolny
Politechnika Koszalinska, Polonya
Karali Patra
Indian Institute Of Technology Patna, Hindistan
Tadeusz Mikolajczyk
Bydgoszcz University Of Science And Technology, Polonya
Daniil Yu Pimenov
South Ural State University, Rusya Federasyonu
Prof. Dr. Murat SARIKAYA Sinop Üniversitesi, Türkiye
Vishal S. Sharma
Dr. B.R. Ambedkar National Institute Of Technology, Hindistan
Makale Türü Açık Erişim Özgün Makale (SSCI, AHCI, SCI, SCI-Exp dergilerinde yayınlanan tam makale)
Dergi Adı International Journal of Advanced Manufacturing Technology (Q2)
Dergi ISSN 0268-3768 Dergi Bilgileri (2019)
Dergi Tarandığı Indeksler SCI-Expanded
Makale Dili İngilizce Basım Tarihi 06-2019
Cilt / Sayı / Sayfa 102 / 9 / 3995–4009 DOI 10.1007/s00170-019-03453-3
Makale Linki http://link.springer.com/10.1007/s00170-019-03453-3
UAK Araştırma Alanları
Üretim Teknolojileri
Özet
The manufacturing of parts from nickel-based superalloy, such as Inconel-800 alloy, represents a challenging task for industrial sites. Their performances can be enhanced by using a smart cutting fluid approach considered a sustainable alternative. Further, to innovate the cooling strategy, the researchers proposed an improved strategy based on the minimum quantity lubrication (MQL). It has an advantage over flood cooling because it allows better control of its parameters (i.e., compressed air, cutting fluid). In this study, the machinability of superalloy Inconel-800 has been investigated by performing different turning tests under MQL conditions, where no previous data are available. To reduce the numerous numbers of tests, a target objective was applied. This was used in combination with the response surface methodology (RSM) while assuming the cutting force input (Fc), potential of tool wear (VBmax), surface …
Anahtar Kelimeler
Inconel-800 | MQL | Optimization | PSO | Sustainable machining | TLBO