| Makale Türü | Özgün Makale (SSCI, AHCI, SCI, SCI-Exp dergilerinde yayınlanan tam makale) | ||
| Dergi Adı | Ceramics International (Q1) | ||
| Dergi ISSN | 0272-8842 Dergi Bilgileri (2021) | ||
| Dergi Tarandığı Indeksler | SCI-Expanded | ||
| Makale Dili | Türkçe | Basım Tarihi | 01-2021 |
| Cilt / Sayı / Sayfa | 47 / 11 / 15542–15560 | DOI | 10.1016/j.ceramint.2021.02.122 |
| Makale Linki | http://dx.doi.org/10.1016/j.ceramint.2021.02.122 | ||
| UAK Araştırma Alanları |
Üretim Teknolojileri
|
||
| Özet |
| Ceramics are widely used in machining of high temperature alloys i.e., Co-based Haynes 25 alloy due to its superior characteristics. The present paper is focused on the performance of whisker-reinforced ceramic cutting tool (WRCCT) under nano-sized solid lubricants dispersed in MQL (nanofluid-MQL) during turning of Co-based Haynes 25 alloy. The turning experiments were performed under several cutting environments (dry, base fluid MQL (BF-MQL), hBN based nanofluid MQL (hBN-NMQL), MoS2 based nanofluid MQL (MoS2-NMQL), graphite based nanofluid MQL Gr-NMQL) by varying cutting speed (200 and 300 m/min) and feed rate (0.1 and 0.15 mm/rev) values. Initially, the viscosity and thermal conductivity of nanofluids were evaluated and then the prepared nanofluids were used for machining experiments. The results reveal that the rate of increase in thermal conductivity coefficient relative to base … |
| Anahtar Kelimeler |
| Haynes 25 superalloy | Nanofluids | Tool wear behaviors | Whisker-reinforced ceramic cutting tool |
| Atıf Sayıları | |
| Web of Science | 66 |
| Scopus | 79 |
| Google Scholar | 100 |
| Dergi Adı | Ceramics International |
| Kısa Adı | CERAM INT |
| Yayıncı | ELSEVIER SCI LTD |
| Açık Erişim | Hayır |
| ISSN | 0272-8842 |
| E-ISSN | 1873-3956 |
| Wos Quartile | Q1 |
| Scopus Quartile | Q1 |
| Tarandığı Indeksler | SCIE , Scopus |
| WoS Kategoriler | MATERIALS SCIENCE, CERAMICS |
| Scopus Kategoriler | CERAMICS AND COMPOSITES | ELECTRONIC, OPTICAL AND MAGNETIC MATERIALS | MATERIALS CHEMISTRY | SURFACES, COATINGS AND FILMS | PROCESS CHEMISTRY AND TECHNOLOGY |